1
|
885062LWS11 PMET 885.062 X LWS30 240 LBS NI-Al WIRE FOR METAL SPRAYING
|
PIONEER HARDFACING PVT LTD
|
M S POLYMET CORP
|
2022-02-16
|
UNITED STATES
|
108.86 KGS
|
2
|
WELDING FLUX TY-SJ102 (CHEMICAL COMPOSITION CAO+MGO 31.7%,AL 2O3+MNO 27.1%,SIO2 +TIO2 24.2%,CAF2 16.0%,S0.011%,P0.058%,H2
|
PIONEER HARDFACING PVT LTD
|
M/S. LAIWU TAISHAN SUNLIGHT WELDING
|
2017-09-21
|
CHINA
|
8.00 MTS
|
3
|
WELDING WIRE- POLYCHROME 100D.109 X DRUM 220(1980 LBS)(CHEMI CAL COMPOSITION:CR 29.0%,C 5.0%, MN 1.7%, SI 0.8%, FE BALANC
|
PIONEER HARDFACING PVT LTD
|
M/S. POLYMET CORPORATION
|
2017-09-11
|
UNITED STATES
|
898.00 KGS
|
4
|
WELDING WIRE-PMET 273.062 X LWS25(150LBS)(CHEMICAL COMPOSITI ON:CR 27.5%,B 3.7%, MN 1.7%, SI 1.6%, FE BALANCE)
|
PIONEER HARDFACING PVT LTD
|
M/S. POLYMET CORPORATION
|
2017-09-11
|
UNITED STATES
|
68.00 KGS
|
5
|
WELDING FLUX TY-SJ102 (CAO+MGO 31.7%,AL2O+MNO 27.1%,SIO2 +TIO2 24.2%,CAF216.0%,S0.011%,P0.058%,H2O 0.010%)
|
PIONEER HARDFACING PVT LTD
|
M/S. LAIWU TAISHAN SUNLIGHT WELDING
|
2017-07-20
|
CHINA
|
6.00 MTS
|
6
|
15CRMO 2.0 MM DIA WELDING WIRE IN 25 KG COIL ( PLAIN BOX ) 2 968/517 C-0.06% SI-0.42% MN-1.05% CR-1.35% MO-.0.48% P-0.016
|
PIONEER HARDFACING PVT LTD
|
M/S. INNOVATIVE ALLOYS SDN BHD
|
2017-06-03
|
MALAYSIA
|
3000.00 KGS
|
7
|
15CRMO -2.0MM DIA WELDING WIRE IN 25 KG COIL(PLAIN BOX)-2958 /417 CHEMICAL COMPOSITION(%)- C-0.06% SI-0.43, MN-1.03, CR-
|
PIONEER HARDFACING PVT LTD
|
M/S. INNOVATIVE ALLOYS SDN BHD
|
2017-06-03
|
MALAYSIA
|
2000.00 KGS
|
8
|
WELDING FLUX TY-SJ102
|
PIONEER HARDFACING PVT LTD
|
M/S. LAIWU TAISHAN SUNLIGHT WELDING
|
2017-05-23
|
CHINA
|
8.00 MTS
|
9
|
WELDING FLUX TY-SJ102
|
PIONEER HARDFACING PVT LTD
|
M/S. LAIWU TAISHAN SUNLIGHT WELDING
|
2017-05-09
|
CHINA
|
5.00 MTS
|
10
|
15CRMO -2.4MM DIA WELDING WIRE IN 25 KG COIL(PLAIN BOX)-2926/417CHEMICAL COMPOSITION(%)- C-0.05, SI-0.40, MN-0.98, CR-1.
|
PIONEER HARDFACING PVT LTD
|
M/S. INNOVATIVE ALLOYS SDN BHD
|
2017-05-08
|
MALAYSIA
|
2500.00 KGS
|