<div style="display:inline;"><img height="1" width="1" style="border-style:none;" alt="" src="//www.googleadservices.com/pagead/conversion/1038283176/?label=gXdMCOiuggIQqOOL7wM&amp;guid=ON&amp;script=0"/></div>

Amg Superalloys Uk Limited S H Bell

US Customs records for Amg Superalloys Uk Limited S H Bell in Baltimore U S A. See their past imports and exports, including shipments from Lanzhou Sihaitong Industrial, a supplier based in China.
Total Shipments
2
Trading Partners
2
Top Partner
LANZHOU SIHAITONG INDUSTRIAL
Ports
2
Top Port
Colon
Contact Info
  • Amg Superalloys Uk Limited S H Bell
    Wh 3501 East Biddle St Baltimore U.S.A. Md 21213

Amg Superalloys Uk Limited S H Bell Records

Get a complete importer history
Updated: 2021-10-11

Total Shipments

2
Date range
Available to paid subscribers
  • 1M
  • 3M
  • 6M
  • 1Y
  • 3Y
  • All
2006-11-01 - 2021-10-11
Total shipments from 2006-11-01 to 2021-10-11
Date range
Available to paid subscribers
Precise data and chart data points are only available to paid subscribers
  • Importer Shipments

Top Ports

Legend
  • Colon
  • Antwerp
More data available to paid subscribers

Sample Shipment From Amg Superalloys Uk Limited S H Bell

Bill of Lading EGLV141100932278
Arrival Date: 2021-10-11
Container Number: TEMU4163043
×
Cargo #1
Description FERRO SILICON ZIRCONIUM FERRO SILICON ZIRCONIUM THE SAME THE SAME THE SAME THE SAME
Keywords ferro silicon zirconium the same HS-Code DATA UNAVAILABLE Piece Count 20
Length 240 Height 102
Width 96 Load Status Loaded
Seal EMCPGZ6710 Equipment Description CN
Type 20 Foot General Purpose Container, Openings at one or both ends Type of Service House to House
Container Type 20 Foot General Purpose Container, Openings at one or both ends Marks & Numbers FESIZR FESIZR 10-50MM NET WEIGHT 1000KGS GROSS WEIGHT 1003KGS BAG NO. 20-1....20-20
More data available to paid subscribers

Related companies to Amg Superalloys Uk Limited S H Bell

LANZHOU SIHAITONG INDUSTRIAL
panama
Sparkline
< 10
Total Shipments
AMG SUPERALLOYS UK LIMITED
belgium
Sparkline
900±
Total Shipments